ASTM B/BM: Standard Specification for Aluminum and Aluminum-Alloy Rivet and Cold-Heading Wire and Rods. See the chemical composition and physical properties of ASTM B Grade O Wrought Aluminium, find alternative materials, and connect with suppliers . See the chemical composition and physical properties of ASTM B Grade T6, find alternative materials, and connect with suppliers.

Author: Fenrill Nelmaran
Country: Denmark
Language: English (Spanish)
Genre: Love
Published (Last): 6 September 2007
Pages: 482
PDF File Size: 7.62 Mb
ePub File Size: 11.55 Mb
ISBN: 293-9-71620-347-7
Downloads: 75409
Price: Free* [*Free Regsitration Required]
Uploader: Arashiktilar

Variations zstm the specified diameter, length, and straightness shall not exceed the permissible variations prescribed. The material shall be supplied in the mill finish and shall conform by the requirements of this specification and shall be commercially sound.

This abstract is a brief summary of the referenced standard. On the other hand, an inspection lot shall consist of an identifiable quantity of material of the same mill form, alloy, temper, and nominal diameter subjected to inspection for non heat-treated tempers.

ASTM B316 Gr 5052 Aluminum Rod

It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application. One tension test per specimen shall be taken.

  JUSTICIA ADHATODA MEDICINAL USES PDF

For heat-treated tempers, an inspection lot shall consist of an identifiable quantity of material of the same mill form, alloy, temper, and nominal diameter traceable to a heat-treat lot or lots, and subjected to inspection at one time. Samples for chemical analysis shall be taken from the material by drilling, sawing, milling, turning, or clipping a representative piece or pieces to obtain a prepared sample.

ASTM does not give any warranty express or implied or make any representation that the contents of this abstract are accurate, complete or up to date. The products covered by this specification shall be produced by extruding, rolling, or drawing, or a combination thereof, at the option of the producer. For rolled or cold-finished wire and rod, see Specification Band for extruded wire and rod, see Specification B Combining values from the two systems may result in non-conformance with the standard.

The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other.

  BOUWAANVRAAG FORMULIER PDF

ASTM B Gr Aluminum Wire at Rs /kilogram | Mumbai | ID:

This specification covers wire and rod in the alloys and the tempers suitable for manufacturing rivets and other similar items by cold-heading operations. Referenced Documents purchase separately The documents listed below are referenced within the subject standard but are not provided as part of the standard.

Link to Active This link will always route to the current Active version of the standard. Throughout this specification the use of the term alloy in the general sense includes aluminum as well as aluminum alloy.

Historical Version s – view previous versions of standard. Resistance to stress corrosion cracking for each lot of specimen shall be established by testing the previously selected tension-test samples for lot acceptance purposes.